Catalogue
Precision alloys
Alloys nichrome-fechral
Cr15Ni60
Cr20Ni30
Cr20Ni80
Cr15AI5
Cr23AI5
Cr23AI5Ti
Cr27AI5Ti
Soft magnetic-alloys
Magnetic-hard alloys
Alloys with a given COTE
Alloys with desired properties of elasticity
Alloys with specific electrical properties
Superconducting alloys
Thermostatic bimetal
Thermocouples
Alumel
Chromel
Kopel
Constantan
Superalloys
Corrosion-resistant alloys
Structural steel
Tool steel
Welding materials
Welding wire
Electrodes